Name: | STROMEYERITE | ||
Specification: | [2], at 298oK | ||
Formula: | AgCuS | ||
Symmetry Class: | orthorhombic | ||
Space Group: | C mc2(1) | ||
Unit Cell Parameters: | a = 4.0590 | b = 6.6170 | c = 7.9670 | ||
Number of Formula Unit: | Z = 4 | Unit Cell Volume, Å3: | Vc = 213.98 |
Number of Atomic Position per full Unit Cell: | P/U = 12 | Molar Volume, cm3/mol: | Vm = 32.22 |
Number of Reflexes used in Structure Determination: | NR = 278 | X-ray density, g/cm3: | p = 6.31 |
R-factor: | R = 0.0610 | MU, 1/cm: | µ = 922.650 |
Wave Length for Calculated Powder Diffraction Patterns: | Cu=1.54056 | Mass attenuation coefficient, cm2/g: | µ/p = 146.129 |
Theta-Interval for CPDP: | T/I = 1-45 |